These crushers are used as a primary stage of aggregate size reduction due to the large feed opening. For these crushers we offer a large range of wear parts to cover all the main needs :
The type of rocks or raw material to be crushed will determine the type of grade we will offer. Generally, for primary crushers, we mainly offer 2 types of grades :
12-14% of Manganese : Non-abrasive area – Soft aggregates (LOS ≥ 25 ≤ 40)
18-20% of Manganese : Abrasive area – Hard aggregates (LOS ≥ 15 ≤ 25).
LOS ANGELES test will allow to measure the choc and wear resistance of the aggregates. If the measured LOS in an area is < to 40, the aggregates are not very resistant to chocs. On the contrary, a measured LOS ≥ to 15, the aggregates are very resistant to the chocs.
*NB : Due to the thickness of the primary jaws, the 21% manganese is not recommended if the abrasiveness of the aggregates is important.